Pemco Frit P-930

Leadless all-fritted base

Alternate Names: Frit 930, Frit P930

OxideAnalysisFormula
CaO5.40%0.289
Na2O4.30%0.209
SrO17.30%0.502
Al2O34.10%0.121
B2O315.40%0.665
SiO252.30%2.616
ZrO21.20%0.029
Oxide Weight300.66
Formula Weight300.66
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.8 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1500-1600F

For cone 06-02, stronita replaces lead in Pb-742. Blends with P-786 for intermediate temperatures.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-930" descrip="Leadless all-fritted base" searchkey="Frit 930, Frit P930" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.300" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="17.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.300" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="1.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved