Pemco Frit P-926

Leadless fast fire frit

Alternate Names: Frit 926, Frit P926

OxideAnalysisFormula
CaO17.00%0.684
K2O0.30%0.007
Na2O8.50%0.309
Al2O35.00%0.111
B2O318.70%0.606
SiO250.50%1.895
Oxide Weight225.57
Formula Weight225.57
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.4 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1650-1700F

Replaced P-54 in wall tile industry. It has lower solubility to prevent thickening or 'set' in glaze slurries.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-926" descrip="Leadless fast fire frit" searchkey="Frit 926, Frit P926" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="17.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved