Pemco Frit P-878

Zirconium opacified frit

Alternate Names: Frit 878, Frit P878

OxideAnalysisFormula
CaO14.60%0.680
Na2O7.60%0.320
B2O317.00%0.638
SiO243.20%1.878
ZrO217.60%0.373
Oxide Weight261.21
Formula Weight261.21
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.9 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1500-1590F

Equivalent to 72.7% P-54 and 27.3% zircon.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-878" descrip="Zirconium opacified frit" searchkey="Frit 878, Frit P878" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.200" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="17.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved