Pemco Frit P-827

Leadless boron free frit for high temperature

Alternate Names: Frit 827, Frit P827

OxideAnalysisFormula
BaO5.50%0.065
CaO13.20%0.427
MgO1.10%0.050
K2O5.00%0.096
Na2O1.40%0.041
ZnO14.40%0.321
Al2O37.90%0.141
SiO251.50%1.555
Oxide Weight181.48
Formula Weight181.48
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.0 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 2000-2040F

For high temperature transparent use 11% clay, 11% silica and 78% frit.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-827" descrip="Leadless boron free frit for high temperature" searchkey="Frit 827, Frit P827" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="5.500" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.400" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="14.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved