Pemco Frit P-802

Leadless flux for cone 06 glazes

Alternate Names: Frit 802, Frit P802

OxideAnalysisFormula
CaO8.90%0.438
K2O6.90%0.202
Na2O8.10%0.360
Al2O39.60%0.260
B2O316.50%0.654
SiO249.90%2.290
Oxide Weight275.56
Formula Weight275.56
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.90
MLRG - Frit Melting Range (C) 1350-1450F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-802" descrip="Leadless flux for cone 06 glazes" searchkey="Frit 802, Frit P802" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="6.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved