Pemco Frit P-786

Leadless all-fritted glaze

Alternate Names: Frit 786, Frit P786

OxideAnalysisFormula
CaO11.50%0.581
K2O3.00%0.090
Na2O2.00%0.091
SrO8.70%0.238
Al2O36.80%0.189
B2O38.80%0.358
SiO259.20%2.790
Oxide Weight283.23
Formula Weight283.23
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.2 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1640-1910F

Used for vitreous and semi-vitreous dinnerwre and artware. Same as Pb-349 with strontia replacing lead. Fires cone 02-8.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-786" descrip="Leadless all-fritted glaze" searchkey="Frit 786, Frit P786" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="8.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved