Pemco Frit P-760

Cadmium bearing frit

Alternate Names: Frit 760, Frit P760

OxideAnalysisFormula
K2O8.10%0.329
Na2O7.30%0.451
CdO7.40%0.220
Al2O34.30%0.161
B2O316.30%0.896
SiO256.60%3.603
Oxide Weight382.62
Formula Weight382.62
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.90
MLRG - Frit Melting Range (C) 1330-1440F

Used in all-fritted glazes with Pb-41 as base for low temperature cadmium-selenium type colors.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-760" descrip="Cadmium bearing frit" searchkey="Frit 760, Frit P760" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.300" tolerance=""/> <oxide symbol="CdO" name="Cadmium Oxide" status="" percent="7.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved