Pemco Frit P-658

Leaded strontium low boron high alumina frit

Alternate Names: Frit 658, Frit P658

OxideAnalysisFormula
CaO4.23%0.330
Li2O0.13%0.020
MgO1.19%0.130
K2O0.86%0.040
Na2O0.56%0.040
SrO3.31%0.140
PbO15.30%0.300
Al2O334.27%1.470
B2O34.93%0.310
SiO235.17%2.560
Oxide Weight437.38
Formula Weight437.38
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-658" descrip="Leaded strontium low boron high alumina frit" searchkey="Frit 658, Frit P658" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.232" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.137" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.198" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.861" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.567" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="3.316" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="15.307" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="34.277" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.932" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="35.172" tolerance=""/> </oxides> </material>