Pemco Frit P-609

LEADLESS FRIT

Alternate Names: Frit 609, Frit P609

OxideAnalysisFormula
CaO7.10%0.321
Li2O1.70%0.145
MgO3.30%0.207
K2O1.10%0.030
Na2O2.20%0.090
SrO8.50%0.208
Al2O38.00%0.199
B2O39.00%0.328
SiO259.10%2.491
Oxide Weight253.36
Formula Weight253.36
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.9 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1430-1530F

Component for partially-fritted leadless glazes firing cone 4-8.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-609" descrip="LEADLESS FRIT" searchkey="Frit 609, Frit P609" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.100" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="1.700" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.200" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="8.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="9.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved