Pemco Frit P-586

Barium, zinc, calcium frit for partially fritted cone 4-10 glazes

Alternate Names: Frit 586, Frit P586

OxideAnalysisFormula
BaO4.10%0.051
CaO14.30%0.481
MgO0.60%0.028
K2O4.00%0.080
Na2O1.60%0.049
ZnO13.40%0.311
Al2O38.20%0.152
B2O34.50%0.122
SiO249.30%1.549
Oxide Weight188.88
Formula Weight188.88
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.5 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1600-1860F
IFP - I.F.P. (celsius) 689C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-586" descrip="Barium, zinc, calcium frit for partially fritted cone 4-10 glazes" searchkey="Frit 586, Frit P586" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.100" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="13.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved