Pemco Frit P-4K47

Strontium sanitaryware hard frit

Alternate Names: 4K47,4K-47

OxideAnalysisFormula
CaO9.70%0.541
K2O1.84%0.061
Na2O2.64%0.133
SrO8.78%0.265
Al2O310.00%0.307
B2O34.96%0.223
SiO262.08%3.230
Oxide Weight312.73
Formula Weight312.73
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.29
GSPT - Frit Softening Point 985C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-4K47" descrip="Strontium sanitaryware hard frit" searchkey="4K47,4K-47" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.700" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.840" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.640" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="8.780" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.960" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.080" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved