Alternate Names: 4K05,4K-05

OxideAnalysisFormula
CaO6.00%0.477
K2O2.80%0.132
Na2O4.60%0.331
ZnO1.10%0.060
Al2O37.60%0.332
B2O313.20%0.845
SiO256.20%4.167
ZrO28.50%0.307
Oxide Weight445.67
Formula Weight445.67
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.54
GSPT - Frit Softening Point 925C

Similar to Fusion Frit FZ-376A, chemistry shown here was copied, not exact.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-4K05" descrip="Moderate melting Zirconia frit" searchkey="4K05,4K-05" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.200" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="8.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved