Pemco Frit P-4D79

Alternate Names: 4D79,4D-79

OxideAnalysisFormula
BaO2.31%0.040
CaO6.77%0.317
MgO0.76%0.050
K2O2.84%0.079
Na2O1.87%0.079
ZnO11.05%0.356
SrO3.12%0.079
Al2O39.23%0.238
B2O36.03%0.228
SiO255.99%2.446
Oxide Weight262.50
Formula Weight262.50
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-4D79" descrip="" searchkey="4D79,4D-79" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.313" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.771" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.760" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.842" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.871" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="11.053" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="3.126" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.233" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.038" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.992" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved