Pemco Frit P-3E12

Semi-opaque all-fritted glaze for cone 02-4

Alternate Names: Frit 3E12, Frit P3E12

OxideAnalysisFormula
CaO6.20%0.284
MgO1.40%0.089
K2O6.70%0.183
Na2O3.00%0.124
ZnO10.10%0.319
Al2O313.20%0.333
B2O34.90%0.181
SiO251.40%2.199
ZrO23.10%0.065
Oxide Weight257.17
Formula Weight257.17
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.80
GSPT - Frit Softening Point 1650F
MLRG - Frit Melting Range (C) 1620-1720F
IFP - I.F.P. (celsius) 658C

A lower-expansion version of P-1J81


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-3E12" descrip="Semi-opaque all-fritted glaze for cone 02-4" searchkey="Frit 3E12, Frit P3E12" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="6.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.400" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="3.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved