Pemco Frit P-311

Calcium borosilicate frit for partially fritted dinnerware glazes

Alternate Names: Frit 311, Frit P311

OxideAnalysisFormula
CaO14.10%0.691
K2O0.70%0.020
Na2O6.50%0.288
Al2O310.00%0.270
B2O314.40%0.569
SiO254.30%2.485
Oxide Weight275.02
Formula Weight275.02
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.0 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1500-1630F
IFP - I.F.P. (celsius) 669C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-311" descrip="Calcium borosilicate frit for partially fritted dinnerware glazes" searchkey="Frit 311, Frit P311" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved