Pemco Frit P-2G63

Highly opaque frit for use in all-fritted cone 06-6 glazes

Alternate Names: 2G63,2G-63

OxideAnalysisFormula
CaO1.50%0.171
MgO0.20%0.032
Na2O7.60%0.782
ZnO0.20%0.016
Al2O35.50%0.344
B2O317.10%1.568
SiO256.60%6.009
ZrO211.30%0.585
Oxide Weight638.01
Formula Weight638.01
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.50
GSPT - Frit Softening Point 1550F
MLRG - Frit Melting Range (C) 1520-1620F
IFP - I.F.P. (celsius) 569C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-2G63" descrip="Highly opaque frit for use in all-fritted cone 06-6 glazes" searchkey="2G63,2G-63" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.600" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="11.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved