Pemco Frit P-238

LEADLESS FRIT

Alternate Names: Frit 238, Frit P238

OxideAnalysisFormula
K2O3.10%0.221
Na2O7.20%0.779
Al2O316.50%1.085
B2O331.70%3.056
SiO241.50%4.633
Oxide Weight670.97
Formula Weight670.97
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.6 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1450-1560F
IFP - I.F.P. (celsius) 535C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-238" descrip="LEADLESS FRIT" searchkey="Frit 238, Frit P238" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="31.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="41.500" tolerance=""/> </oxides> </material>