Pemco Frit P-1V04

High sodium low boron low alumina body and glaze flux

Alternate Names: 1V-04,1V04

OxideAnalysisFormula
CaO6.30%0.293
K2O2.30%0.064
Na2O15.30%0.643
Al2O33.70%0.095
B2O32.60%0.097
SiO269.80%3.028
Oxide Weight260.76
Formula Weight260.76
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.9x10-6 (50-450C)
GSPT - Frit Softening Point 1450F
MLRG - Frit Melting Range (C) 1400-1550F
IFP - I.F.P. (celsius) 605C

Alkaline-borate flux normally used in wall tile glazes at Cone 1. Sometimes used as engobe or body flux.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1V04" descrip="High sodium low boron low alumina body and glaze flux" searchkey="1V-04,1V04" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved