Pemco Frit P-1T27

High expansion zirconia fluorine frit

Alternate Names: 1T-27,1T27

OxideAnalysisFormula
CaO4.80%0.249
Na2O13.40%0.629
ZnO3.40%0.122
F9.80%1.502
Al2O37.40%0.211
B2O318.20%0.761
SiO227.40%1.327
ZrO213.10%0.310
Oxide Weight283.88
Formula Weight283.88
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 12.10
GSPT - Frit Softening Point 1300F
MLRG - Frit Melting Range (C) 1250-1350F
IFP - I.F.P. (celsius) 475C

Used in satin matte crackle glazes at Cone 06


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1T27" descrip="High expansion zirconia fluorine frit" searchkey="1T-27,1T27" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.400" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="3.400" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="9.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="27.400" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="13.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved