Pemco Frit P-1R63

Alternate Names: 1R-63,1R63

OxideAnalysisFormula
CaO14.30%0.671
K2O0.40%0.011
Na2O7.50%0.318
Al2O34.40%0.113
B2O316.60%0.627
SiO246.70%2.044
ZrO29.60%0.205
Oxide Weight261.76
Formula Weight261.76
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.80
GSPT - Frit Softening Point 1550F
MLRG - Frit Melting Range (C) 1500-1600F
IFP - I.F.P. (celsius) 662C

Similar to P-926 containing 10% zirconia


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1R63" descrip="" searchkey="1R-63,1R63" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.700" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved