Pemco Frit P-1J81

Semi-opaque all-fritted glaze for cone 02-4

Alternate Names: P1J81,1J-81

OxideAnalysisFormula
CaO5.10%0.235
MgO0.60%0.038
K2O8.60%0.236
Na2O4.50%0.187
ZnO9.60%0.304
Al2O313.40%0.339
B2O34.80%0.178
SiO250.30%2.159
ZrO23.20%0.067
Oxide Weight258.25
Formula Weight258.25
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.40
GSPT - Frit Softening Point 1620F
MLRG - Frit Melting Range (C) 1580-1680F
IFP - I.F.P. (celsius) 610C

Add 10% clay.
Generally used with additional zirconium silicate opacifier. This glaze has excellent gloss and smoothness at Cone 02 through Cone 1.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1J81" descrip="Semi-opaque all-fritted glaze for cone 02-4" searchkey="P1J81,1J-81" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.500" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="9.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.300" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="3.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved