Pemco Frit P-1F07

High CaO/Na2O/ZnO borosilicate low alumina frit

Alternate Names: 1F07,1F-07

OxideAnalysisFormula
BaO3.70%0.042
CaO14.30%0.444
MgO0.40%0.017
K2O1.10%0.020
Na2O9.60%0.269
ZnO9.70%0.207
Sb2O30.10%0.001
Al2O34.30%0.073
B2O320.20%0.505
SiO236.10%1.045
Oxide Weight173.15
Formula Weight173.15
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.30
GSPT - Frit Softening Point 1450F
MLRG - Frit Melting Range (C) 1380-1540F
IFP - I.F.P. (celsius) 690C

For partially-fritted textured glazes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1F07" descrip="High CaO/Na2O/ZnO borosilicate low alumina frit" searchkey="1F07,1F-07" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="3.700" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="9.700" tolerance=""/> <oxide symbol="Sb2O3" name="Antimony Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="20.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved