Pemco Frit P-1A44

Low expansion high zinc high boron frit

Alternate Names: 1A44,1A-44

OxideAnalysisFormula
ZnO59.50%1.000
B2O332.50%0.639
SiO28.00%0.182
Oxide Weight136.81
Formula Weight136.81
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 4.60
GSPT - Frit Softening Point 1400F
MLRG - Frit Melting Range (C) 1350-1450F
IFP - I.F.P. (celsius) 660C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1A44" descrip="Low expansion high zinc high boron frit" searchkey="1A44,1A-44" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="59.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="32.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="8.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved