Pemco Frit P-1409

Low expansion high magnesia alkali-free leadless glaze frit

Alternate Names: Frit 1409, Frit P1409

OxideAnalysisFormula
CaO2.20%0.132
MgO10.40%0.868
Al2O314.40%0.475
B2O329.00%1.402
SiO244.00%2.463
Oxide Weight336.38
Formula Weight336.38
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 4.7x10-6 (50-450C)
MLRG - Frit Melting Range (C) 1750-1850F
IFP - I.F.P. (celsius) 694C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit P-1409" descrip="Low expansion high magnesia alkali-free leadless glaze frit" searchkey="Frit 1409, Frit P1409" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="10.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="14.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved