Pearl Ash Calcined

Pure source of K2O

Formula: K2O
Alternate Names: Potash Calcined, Calcined Potash

OxideAnalysisFormula
K2O100.00%1.000
Oxide Weight94.20
Formula Weight94.20
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pearl Ash Calcined" descrip="Pure source of K2O" searchkey="Potash Calcined, Calcined Potash" loi="0.00" casnumber="584-08-7"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="100.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved