Pastelle BY Ball Clay

OxideAnalysisFormula
K2O1.60%0.056
Na2O0.20%0.011
TiO21.20%0.049
Al2O331.20%1.000
SiO254.00%2.937
Fe2O31.10%0.022
LOI10.00
Oxide Weight291.94
Formula Weight324.38
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pastelle BY Ball Clay" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="31.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="10.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved