P4 Quartz

OxideAnalysisFormula
CaO0.04%0.145
K2O0.10%0.217
TiO20.03%0.077
Al2O30.50%1.000
SiO299.10%336.379
Fe2O30.04%0.051
LOI0.20
Oxide Weight20361.24
Formula Weight20402.04
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.6
HMOH - Hardness (Moh) 7
BDGC - Bulk Density g/cc (Packed) 1.2
UPSD - Ultimate Particle Size Distribution >71 micron: 1.6%
pHPW - pH for dry powder 8-9

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="P4 Quartz" descrip="" searchkey="" loi="0.00" casnumber="87347-84-0"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.040" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.030" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="99.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.040" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved