Opeal OP-5 Ball Clay

Super-white ball clay

OxideAnalysisFormula
CaO0.05%0.003
MgO0.10%0.008
K2O1.21%0.042
Na2O0.15%0.008
TiO20.54%0.022
Al2O331.20%1.000
SiO253.12%2.890
Fe2O30.92%0.019
LOI12.80
Oxide Weight285.37
Formula Weight327.26
If this formula is not unified correctly please contact us.

Based on OP-4 but improved to meet customers ' demand, low cost of producing, excellent plasticity and excellent whiteness after burning.
Application in high-grade polished tiles, porcelain tiles, sanitary ware, ceramic glaze.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Opeal OP-5 Ball Clay" descrip="Super-white ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.050" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.210" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.150" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.540" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="31.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.120" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.920" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="12.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved