Opeal OP-4 Ball Clay

Super-white ball clay

OxideAnalysisFormula
CaO0.07%0.004
MgO0.10%0.008
K2O1.12%0.038
Na2O0.09%0.005
TiO20.54%0.022
Al2O331.80%1.000
SiO252.89%2.823
Fe2O30.88%0.018
LOI12.51
Oxide Weight280.63
Formula Weight320.75
If this formula is not unified correctly please contact us.

Developed according to high broken rate as lacking raw material of clay. It has outsanding plasticity and may lower the broken rate of semi-finished ceramic products. Good whiteness after 1220C; burning. Application high-grade polished tiles, sanitary ware, ceramic glaze,etc.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Opeal OP-4 Ball Clay" descrip="Super-white ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.070" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.120" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.090" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.540" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="31.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.890" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.880" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="12.510" tolerance=""/> </volatiles> </material>