Opeal OP-3 Ball Clay

Super-white ball clay

OxideAnalysisFormula
CaO0.06%0.003
MgO0.08%0.006
K2O1.26%0.040
Na2O0.11%0.005
TiO20.43%0.016
Al2O334.20%1.000
SiO250.60%2.511
Fe2O30.72%0.013
LOI12.54
Oxide Weight260.85
Formula Weight298.25
If this formula is not unified correctly please contact us.

Excellent plasticity and reasonable particle distribution and it can improve the speed and quality when making semi-finished ceramic products. Application in high-grade polished tiles, porcelain tiles, sanitary ware,etc .


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Opeal OP-3 Ball Clay" descrip="Super-white ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.060" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.080" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.260" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.110" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.430" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="34.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.720" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="12.540" tolerance=""/> </volatiles> </material>