Opeal OP-1 Ball Clay

Super-white ball clay

OxideAnalysisFormula
CaO0.02%0.001
MgO0.03%0.003
K2O0.45%0.017
Na2O0.10%0.006
TiO20.33%0.015
Al2O328.52%1.000
SiO260.47%3.598
Fe2O30.28%0.006
LOI9.80
Oxide Weight322.59
Formula Weight357.64
If this formula is not unified correctly please contact us.

Developed according to current popular Super-white polished tiles and high-grade tableware. This product has a outstanding whiteness after burning(whiteness above 90 degree after 1220℃ burning) and it shows the best level in refined ball clay field.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Opeal OP-1 Ball Clay" descrip="Super-white ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.020" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.030" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.450" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.330" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="28.520" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.470" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.280" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="9.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved