Old Hickory No. 2 Ball Clay

Legacy ball clay

OxideAnalysisFormula
CaO0.10%0.005
MgO0.20%0.015
K2O0.20%0.006
Na2O0.10%0.005
TiO21.30%0.049
Al2O333.70%1.000
SiO251.60%2.599
Fe2O30.80%0.015
LOI11.00
Oxide Weight266.35
Formula Weight299.27
If this formula is not unified correctly please contact us.
L5M - % < 0.5 microns 43%
WABS - Water absorption Cone 9: 7.8%
FSHR - Firing Shrinkage Cone 9: 6.0%
DSHR - Drying Shrinkage 7.6%
MOR5 - Dry M.O.R. (50% Silica) 380 psi

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Old Hickory No. 2 Ball Clay" descrip="Legacy ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="33.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.800" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="11.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved