Old Hickory FC340 Ball Clay

Alternate Names: FC-340 Ball Clay

Oxide Analysis Formula
SiO2 62.04% 4.37
Al2O3 24.10% 1.00
Fe2O3 1.01% 0.03
TiO2 1.27% 0.07
CaO 0.05% 0.00
MgO 0.30% 0.03
K2O 1.18% 0.05
Na2O 0.11% 0.01
LOI9.94%
Oxide Weight 381.17
Formula Weight 423.24

Notes

It is an equivalent to CDI ball clay used in talc casting slips.
It is a little more plastic that KT#1-4.

Related Information

Links

URLs http://www.oldhickoryclay.com/FC-340.htm
FC-340 Data Sheet
Materials Ball Clay
Suppliers Old Hickory
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved