Ocmulgee Red Clay

HIGH IRON CLAY

OxideAnalysisFormula
CaO0.37%0.031
MgO0.79%0.092
K2O1.29%0.064
Na2O0.36%0.027
TiO21.20%0.070
Al2O321.80%1.000
SiO253.90%4.196
Fe2O36.40%0.187
MnO0.23%0.015
LOI13.70
Oxide Weight403.98
Formula Weight468.11
If this formula is not unified correctly please contact us.

A sandy, coarse, iron bearing sedimentary clay. Used in brick and pipe manufacture.
No longer available.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ocmulgee Red Clay" descrip="HIGH IRON CLAY" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.370" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.790" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.290" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.360" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="6.400" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.230" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="13.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved