Nyad 325 Wollastonite

Alternate Names: Nyad-200 Wollastonite

OxideAnalysisFormula
CaO46.36%0.995
MgO0.15%0.004
K2O0.02%0.000
TiO20.05%0.001
Al2O30.40%0.005
SiO251.60%1.034
Fe2O30.77%0.006
MnO0.15%0.003
LOI0.50
Oxide Weight119.83
Formula Weight120.44
If this formula is not unified correctly please contact us.

A North American Wollastonite.
This is the Nyad grade used most commonly in ceramic glazes.

Appearance: White
Shape: Acicular
Specific gravity: 2.9
Refractive Index: 1.63
GE Brightness: 90
pH (aqueous solution): 9.9
Water solubility (gms./100cc): 0.0095
Density (lbs./cu.ft.): 181 (2.9 g/cc)
Moh's hardness: 4.5
Coefficient of expansion: (in/in/degree C): 6.5 x 10 -8
Melting point: 1410
on 325# sieve: 1% (Vansil W-30: 0.05%)
Hegman Fineness of Grain: 3 (Vansil W-30: 4)
Median Particle Size: 14
Surface Area (m2/g) (BET): 1.5
LOI (1000C): 0.5% (Vansil: 1.6%)


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Nyad 325 Wollastonite" descrip="" searchkey="Nyad-200 Wollastonite" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="46.360" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.150" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.020" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.050" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.770" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.150" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved