#1 Q-Rok

30 mesh silica

OxideAnalysisFormula
SiO298.00%1.000
LOI0.50
Oxide Weight60.10
Formula Weight60.40
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="#1 Q-Rok" descrip="30 mesh silica" searchkey="" loi="0.00" casnumber="7631-86-9"> <oxides> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="98.000" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.500" tolerance=""/> </volatiles> </material>