Noor Albite

Alternate Names: Egyptian Albite, Elnaba Valley Albite

OxideAnalysisFormula
CaO0.22%0.025
MgO0.01%0.002
K2O2.63%0.179
KNaO10.53%0.863
Al2O315.94%1.000
SiO272.26%7.694
Fe2O30.25%0.010
Oxide Weight651.67
Formula Weight651.67
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Noor Albite" descrip="" searchkey="Egyptian Albite, Elnaba Valley Albite" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.220" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.010" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.630" tolerance=""/> <oxide symbol="KNaO" name="Potassium/Sodium Oxides" status="" percent="10.530" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="15.940" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="72.260" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.250" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved