Nickel Oxide Green

Formula: NiO
Alternate Names: NiO, Nickelous oxide, Green Nickel Oxide, Nickel(II) oxide

OxideAnalysisFormula
NiO100.00%1.000
Oxide Weight74.70
Formula Weight74.70
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 6.6- 7.5
GSPT - Frit Softening Point 1984C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Nickel Oxide Green" descrip="" searchkey="NiO, Nickelous oxide, Green Nickel Oxide, Nickel(II) oxide" loi="0.00" casnumber="34492-97-2"> <oxides> <oxide symbol="NiO" name="Nickel Oxide" status="" percent="100.000" tolerance=""/> </oxides> </material>