OxideAnalysisFormula
CaO0.21%0.015
MgO0.12%0.012
K2O0.78%0.034
Na2O0.20%0.013
TiO20.84%0.043
Al2O324.95%1.000
SiO260.34%4.105
Fe2O31.42%0.036
MnO0.03%0.002
LOI11.11
Oxide Weight363.40
Formula Weight408.82
If this formula is not unified correctly please contact us.

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="New FHC" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.210" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.120" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.780" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.840" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="24.950" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.340" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.420" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.030" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="11.110" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved