Na & Ca Metasilicate Eutectic

Formula: 3.8Na2SiO3 . CaSiO3

OxideAnalysisFormula
CaO9.60%0.207
Na2O40.60%0.793
SiO249.80%1.003
Oxide Weight121.07
Formula Weight121.07
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 932C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Na & Ca Metasilicate Eutectic" descrip="" searchkey="" loi="0.00" casnumber="n/a"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="40.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved