Na & Ba Metasilicate Eutectic

Formula: BaSiO3 . 2.62Na2SiO3

OxideAnalysisFormula
BaO28.70%0.276
Na2O30.40%0.724
SiO240.90%1.004
Oxide Weight147.59
Formula Weight147.59
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 908C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Na & Ba Metasilicate Eutectic" descrip="" searchkey="" loi="0.00" casnumber="n/a"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="28.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="30.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved