N6640

Alkaliborsilikat

OxideAnalysisFormula
K2O0.50%0.362
Na2O0.20%0.220
ZnO0.50%0.419
Al2O30.15%0.100
B2O30.30%0.294
SiO22.00%2.267
Oxide Weight248.70
Formula Weight248.70
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 119
GSPT - Frit Softening Point 560C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="N6640" descrip="Alkaliborsilikat" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.150" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="2.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved