Mullite Fused Dense

ELTRO FUSED MULLITE

OxideAnalysisFormula
CaO0.05%0.001
MgO0.05%0.002
K2O0.15%0.002
Na2O0.15%0.003
TiO20.01%0.000
Al2O376.30%1.000
SiO223.30%0.518
Fe2O30.05%0.000
Oxide Weight133.76
Formula Weight133.76
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 3.14

Particle Size: 0.7-1.5mm
Free iron grains: .02% max
Grain porosity: 2%
Bulk density: 2.09 g/cm3
Refractoriness: 1900C

Also available in sizes: 0.125-0.25mm, 0.25-0.5mm, 0.5-1.0mm for precision metal casting industry and -45 micron for use as a face coat.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Mullite Fused Dense" descrip="ELTRO FUSED MULLITE" searchkey="" loi="0.00" casnumber="55964-99-3"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.050" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.050" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.150" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.150" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.010" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="76.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="23.300" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.050" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved