Mullite 73 Sintered

OxideAnalysisFormula
CaO0.05%0.001
MgO0.15%0.005
K2O0.80%0.012
Na2O0.30%0.007
TiO20.20%0.003
Al2O373.30%1.000
SiO224.70%0.572
Fe2O30.50%0.004
Oxide Weight139.15
Formula Weight139.15
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 3.13

Particle Size: 1.5-3.0mm
Free iron grains: .02% max
Grain porosity: 3%
Bulk density: 2.89 g/cm3
Refractoriness: 1875/1900C


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Mullite 73 Sintered" descrip="" searchkey="" loi="0.00" casnumber="55964-99-3"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.050" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.150" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="73.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="24.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved