Mullite 63 Sintered

OxideAnalysisFormula
CaO0.10%0.003
MgO0.20%0.008
K2O1.20%0.020
Na2O0.20%0.005
TiO20.20%0.004
Al2O363.70%1.000
SiO233.60%0.895
Fe2O30.70%0.007
Oxide Weight159.97
Formula Weight159.97
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 3.02

Particle Size: 0-0.7mm
Free iron grains: .02% max
Grain porosity: 3%
Bulk density: 2.74 g/cm3
Refractoriness: >1800C


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Mullite 63 Sintered" descrip="" searchkey="" loi="0.00" casnumber="55964-99-3"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="63.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="33.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved