Mulcoa 47 Calcine Grog

Mullite grog

OxideAnalysisFormula
TiO21.90%0.052
Al2O346.80%1.000
SiO250.00%1.813
Fe2O30.95%0.013
Oxide Weight217.19
Formula Weight217.19
If this formula is not unified correctly please contact us.

A number of grades are available and are used in the refractory industry.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Mulcoa 47 Calcine Grog" descrip="Mullite grog" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="46.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.950" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved