Moulin Fritte M95

Fritte au zinc

OxideAnalysisFormula
MgO3.00%0.120
Na2O4.00%0.104
ZnO39.00%0.775
Al2O36.00%0.095
SiO240.00%1.077
Oxide Weight148.85
Formula Weight148.85
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 590C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Moulin Fritte M95" descrip="Fritte au zinc" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="39.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved