Moulin Fritte M85

Fritte boro-alcaline

OxideAnalysisFormula
BaO37.00%0.681
Na2O7.00%0.319
SiO256.00%2.630
Oxide Weight282.28
Formula Weight282.28
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 505C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Moulin Fritte M85" descrip="Fritte boro-alcaline" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="37.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved