Moulin Fritte M759

Fritte boro-alcaline

OxideAnalysisFormula
Na2O15.00%1.000
Al2O351.00%2.067
SiO234.00%2.338
Oxide Weight413.33
Formula Weight413.33
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 548C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Moulin Fritte M759" descrip="Fritte boro-alcaline" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="51.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="34.000" tolerance=""/> </oxides> </material>