OxideAnalysisFormula
PbO62.30%1.000
B2O329.30%1.508
SiO28.40%0.501
Oxide Weight358.27
Formula Weight358.27
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 495C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Moulin Fritte M460" descrip="Fritte plombo-boracique" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="62.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="8.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved